耐候性試驗(yàn)
Weathering Testing咨詢熱線
18566398802JIS K6259是關(guān)于《硫化橡膠和熱塑性橡膠 耐臭氧性能測(cè)定》的測(cè)試方法。以下為部分英文標(biāo)準(zhǔn)原文,出于版權(quán)保護(hù),如需JIS K6259標(biāo)準(zhǔn)全文或JIS K6259中文版本標(biāo)準(zhǔn),請(qǐng)垂詢客服人員。
This Japanese Industrial Standard specifies the testing methods t o measure the resistance to ozone cracking for vulcanized rubber.
Remarks 1 The standards cited in this Standard are listed as follows:
JIS K 6200 Glossary of terms used in rubber industry
JIS K 6250 General rules of physical testing methods for rubber,vulcanized or thermoplastic
JIS K 6251 Tensile testing methods for vulcanized rubber
JIS K 8001 General rule for test methods of reagents
JIS K 8637 Sodium thiosulfate pentahydrate
JIS K 8913 Potassium iodide
JIS K 9007 Potassium dihydrogenphosphate
JIS K 9019 Disodium hydrogenphosphate 12-water
2 The International Standards corresponding to this Standard are listed as follows:
IS0 1431-1:1989 Rubber, vulcanized or thermoplastic - Resistance to ozone cracking - Part 1 :Static strain test
ISOIDIS 1431-2:1992 Rubber, vulcanized - Resistance to ozone cracking - Part 2 :Dynamic strain test
3 The units and numerical values given in ( 1 in this Standard are based on the traditional units, and are standard values. However,traditional units becomes an informative reference on and afterApril Ist, 1995.
For the purposes of this Standard, the definitions given in JIS K 6200 and the following definitions apply.
(1)critical strain The maximum tensile strain, which has no cracking, given when test piece has been exposed in specified ozone-concentrated atmosphere at specified temperature for specified duration.
(2)limiting strain The maximum tensile strain given when the duration needed for cracking on a test piece is very long, and when the occurring time of its cracking cannot be forecasted.
(3)static ozone-crackingtest When a test piece, under a static tensile strain,is exposed in the air containing an artificially prepared low concentrated ozone,the test to evaluate the condition of cracking, the duration needed to make cracking, or the maximum tensile strain by which no cracking takes place.
(4)dynamic ozone-cracking test When a test piece is exposed in the air containing an artificially prepared low concentrated ozone while dynamic tensile strain is applying on the test piece, the test to evaluate the condition of cracking and the duration by which cracking takes place
以下標(biāo)準(zhǔn)信息來自互聯(lián)網(wǎng)搜索整理,僅供學(xué)習(xí)使用,可以免費(fèi)下載。
歡迎了解專業(yè)工程師提供的JIS K6259-2004標(biāo)準(zhǔn)解讀,請(qǐng)加微信。
溫馨提醒:本JIS K6259-2004可能存在更新的版本,建議尋找JIS K6259-2004的發(fā)行商確認(rèn)。
SIM 7500臭氧加速老化箱為用戶測(cè)試橡膠產(chǎn)品的臭氧老化提供了可靠的測(cè)試條件。
SIM 7500 馬上詢價(jià)SIM 6010-T耐臭氧老化試驗(yàn)箱用于紡織工業(yè),造紙工業(yè)等其他科學(xué)實(shí)驗(yàn)。
SIM 6010T 馬上詢價(jià)SIM 6300專門用于電纜和密封件的測(cè)試:自動(dòng)PLC控制,精確模擬和控制溫度、濕度、臭氧濃度。
SIM 6300 馬上詢價(jià)